@article{oai:kitami-it.repo.nii.ac.jp:00006513, author = {梅沢, 利二 and 矢郎, 幸保 and 千葉, 富久男}, issue = {2}, journal = {北見工業大学研究報告}, month = {Mar}, note = {application/pdf, Studies on semiconductor-liquid junction solar cells were performed with a polycrystaline n-TiO_2/NaOH//H_2SO_4,/Pt system. The polycrystalline n-TiO_2 (rutile) was formed by heat oxidation in air of 10^<-3> Torr at 900℃ for several different heating times. The most efficient polycrystaline n-TiO_2 was obtained by heat oxidation of 90 minutes, and the cell made of this n-TiO_2 produced the highest maximum power of the 1 N NaOH/1 N H_2SO_4 solution. For further development of this type, a semiconductor having a smaller band-gap should be used instead of, n-TiO_2. This must be stable in electrolyte solutions A-silicon will be investigated in further studies, we planning in the near future.}, pages = {209--219}, title = {半導体一液体接合型太陽電池の基礎的研究 1.多結晶酸化チタン半導体電極を用いた場合の特性}, volume = {12}, year = {1981} }